SINO铁精矿提铁降杂精选试验研究  

Study of Iron Concentrate Separation Tests to Reduce Impurity and Improve Ore Quality in Sino Iron Ore Project

在线阅读下载全文

作  者:侯柠 祝昕冉 

机构地区:[1]中冶北方技术有限公司,辽宁大连116600 [2]东北大学资源与土木工程学院,辽宁沈阳110004

出  处:《矿业工程》2015年第1期21-23,共3页Mining Engineering

摘  要:研究了澳大利亚SINO铁精矿的物理、化学性质,并对该铁精矿进行了提铁降杂精选磁选试验。在控制磁场强度1 400Oe;选别磁场强度1 300Oe,给矿量60kg/h,溢流量1 044L/h,底流量46.8L/h的条件下,可获得品位69.38%,回收率95.72%的精矿产品。Physical and chemical properties of iron concentrates in SINO Iron Project in Australia are studied and magnetic separation tests of concentrates to improve ore quality and reduce impurity are conducted. Under the condition that intensity of controlling magnetic field is 1 400 Oe, intensity of separation magnetic field is 1 3000e, ore feed is 60 kg/h, overflow rate is 1 044L/h and underflow rate is 46.8L/h, concentrates with 69.38% grade and 95.72% recovery can be obtained.

关 键 词:SINO铁精矿 提铁降杂 磁选 精选 

分 类 号:TD913[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象