某高砷难处理金精矿回收有价元素试验  被引量:4

Test of Recovery of Valuable Metals from High Arsenic-bearing Gold Concentrate

在线阅读下载全文

作  者:黄海辉[1] 徐晓辉[1] 王云[1] 袁朝新[1] 郭持皓[1] 常耀超[1] 孙留根[1] 

机构地区:[1]北京矿冶研究总院,北京100160

出  处:《有色金属(冶炼部分)》2015年第4期44-46,58,共4页Nonferrous Metals(Extractive Metallurgy)

基  金:国家重大科学仪器设备开发专项(012YQ22011905)

摘  要:采用两段焙烧—酸浸—氰化浸出工艺从某高砷难处理金精矿中回收有价金属。结果表明,一段焙烧温度550℃,二段焙烧温度630℃,酸浸时间90min,控制终点pH 1.0时,铜浸出率达到82.44%;酸浸渣细磨至-0.039mm占88.9%,氰化钠用量6kg/t,氰化浸出48h,金浸出率达到90.98%。Valuable metals were recovered from high arsenic-bearing gold concentrate by processes of two-stage roasting, acid leaching, and cyanide leaching. The results show that copper leaching rate is 82.44% under the optimum conditions including first-stage roasting temperature of 550 ℃, second-stage roasting temperature of 630 ℃, acid leaching time of 90 rain and terminal pH value of 1.0. Acidic leaching residue is cyanide leached with gold leaching rate of 90.98% under the conditions including grain size of 88.9% - 0. 039 mm, dosage of sodium cyanide of 6 kg/t, and cyanide leaching time of 48 h.

关 键 词:高砷金精矿 两段焙烧 酸浸 氰化   

分 类 号:TF831[冶金工程—有色金属冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象