某钒钛磁铁矿尾矿中钛铁矿的选矿研究  被引量:12

Study on recovering ilmenite from V-Ti magnetite tailings

在线阅读下载全文

作  者:刘长淼[1,2] 吴东印[1,2] 吕子虎[1,2] 赵登魁[1,2] 卫敏[1,2] 王守敬[1,2] 冯安生[1,2] 郭珍旭[1,2] 

机构地区:[1]中国地质科学院郑州矿产综合利用研究所,河南郑州450006 [2]国土资源部多金属矿评价与综合利用重点实验室,河南郑州450006

出  处:《中国矿业》2015年第5期115-117,128,共4页China Mining Magazine

基  金:国土资源部地质矿产评价专项项目资助(编号:12120113088200);国家自然科学基金项目资助(编号:U1304519);中国地质调查局百名青年地质英才培养计划资助

摘  要:某钒钛磁铁矿尾矿品位较低,TiO2品位为3.2%,试样中钛铁矿的含量为5%。试样中TiO2在细级别中分布较多。试样经磁选预选可有效的抛除大量尾矿,钛粗精矿经分级后的重选效果较好,然后采用高压电选工艺,可获得品位大于38%的钛精矿。"磁选-重选-电选"综合条件试验可获得TiO2品位为39.28%,回收率13.87%的钛精矿。A certain V-Ti magnetite tailing is of the type of low grade sample .The grade of TiO2 in the sample is 3 .2% ,and the content of ilmenite in the sample is 5% .TiO2 is mainly distributed in the fine sample .After discarding tailings by magnetic separation ,rough concentrate with the TiO2 grade of 12% was obtained .Then rough concentrate was classficated to carry on the gravity and electrostatic separation ,and concentrate with TiO2 grade of 38% was gained .Based on the process of “magnetic-gravity-electrostatic separation” ,the grade of TiO2 in final concentration is 39 .28% ,and the recovery rate of TiO2 is 13 .87% .

关 键 词:尾矿 钛铁矿 强磁抛尾 重选 电选 

分 类 号:TD923.13[矿业工程—选矿]

 