作 者:黄红军[1] 杜志鸿[1] 胡建伟[1] 王晓梅[1] 万红敬[1] 王建江[1]
机构地区:[1]军械工程学院,石家庄050003
出 处:《包装工程》2015年第13期1-4,共4页Packaging Engineering
基 金:国家自然科学基金(51103178)
摘 要:目的制备一种性能优良的黏性泡沫材料。方法采用分步法制备环氧树脂共混改性聚氨酯泡沫材料,研究泡沫材料粘附性能变化规律及环氧树脂质量分数对材料粘附性能的影响。对共混改性的环氧树脂/聚氨酯泡沫材料进行粘附性能测定、内部结构以及热稳定性表征。结果环氧树脂的质量分数对聚氨酯泡沫材料的粘附性能有很大影响。结论在环氧质量分数为50%时,泡沫材料具有较好粘附性能和热稳定性,材料内部形成了互穿程度良好的互穿聚合物网络结构。This research aimed to produce foams with properties of good adhesion. Blend-modified epoxy/polyurethane foam was synthesized by step-preparation method. The effect of epoxy mass fraction on the foam adhesion and the changing pattern of adhesion property were studied. The performance of adhesion, internal structure and thermal stability of the foam were characterized. The results showed that the mass fraction of epoxy had great effect on the adhesion property of the foam. The optimal adhesive property and the thermal stability were obtained when the mass fraction of epoxy was 50%, and the epoxy/polyurethane foam developed a structure of interpenetrating polymer networks.
分 类 号:TB484.3[一般工业技术—包装工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.171