检索规则说明:AND代表“并且”;OR代表“或者”;NOT代表“不包含”;(注意必须大写,运算符两边需空一格)
检 索 范 例 :范例一: (K=图书馆学 OR K=情报学) AND A=范并思 范例二:J=计算机应用与软件 AND (U=C++ OR U=Basic) NOT M=Visual
机构地区:[1]河南机电高等专科学校计算机科学与技术系,河南新乡453002 [2]郑州大学材料科学与工程学院,河南郑州450000
出 处:《铸造技术》2015年第8期1967-1969,共3页Foundry Technology
基 金:河南省教育厅科学技术重点研究资助项目(13A520221;14A520045)
摘 要:研究了GH3030合金在0.1和-1.0应变比下的高温低周疲劳行为。结果表明,应变高时会有循环硬化出现,应变低时会先软化后硬化。两种应变比下有比较接近的应变滞后回线,并且高温低周疲劳寿命差别也不明显。不论应变比是多少,都有轮胎花样出现。The high-temperature low-cycle fatigue behavior of the alloy GH3030 under the strain ratio of 0.1 and-1.0 was investigated. The results show that cycle hardening appears for the alloy GH3030 under a high stain, while the softening at first and then hardening appears under a low stain. The strain hystersis curves of the samples under the two strain ratios are similar, and the high-temperature low-cycle fatigue lives under the two cases are also comparable. Moreover, the tire pattern will appear no matter the strain ratio.
分 类 号:TG132.3[一般工业技术—材料科学与工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.28