铁水包加盖设备改造实践  被引量:5

Reformation practice of the capped iron ladle

在线阅读下载全文

作  者:项宝胜 

机构地区:[1]首钢京唐钢铁联合有限责任公司设备部,河北唐山063200

出  处:《中国冶金》2015年第9期37-40,共4页China Metallurgy

摘  要:介绍了铁水包加盖设备在首钢京唐公司的应用实践,铁水包加盖可以减少铁水在运输过程中的温度损失,加盖后比加盖前平均温降减低17.4℃,达到了预期目标。铁水包加盖基本可以实现全程的铁水红包运行,加盖后对空包散热起到了较好的抑制作用,减少温降对耐火材料的侵蚀,铁水包加盖后铁水包平均寿命有了较大幅度的提升,可见铁水包加盖对耐火材料寿命的提高效果显著。The application practice of the capped iron ladle at Shougang Jingtang company is introduced. The capped iron ladle can reduce the molten iron temperature loss by 17.4 ℃ on average during the transportation and the expected goal is achieved. The capped iron ladle can realize the hot ladle running throughout the transport. Since the capped iron ladle provides a better insulation protection for the empty ladle heat, the refractory erosion caused by the temperature drop can be reduced, thus the average life of the iron ladle has been greatly improved. Clearly it has an obvious effect on the refractory life improvement.

关 键 词:铁水包加盖 实践 温降 耐火材料寿命 

分 类 号:TF341.4[冶金工程—冶金机械及自动化]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象