柔性憎水型瓷砖填缝剂的研制  被引量:1

Preparation of flexible hydrophobic mortar for gap filler of ceramic wall

在线阅读下载全文

作  者:战美秋[1] 张万喜[2] 

机构地区:[1]吉林建筑大学土木工程学院,吉林长春130000 [2]吉林大学材料科学与工程学院,吉林长春130000

出  处:《四川建筑科学研究》2015年第5期131-134,共4页Sichuan Building Science

摘  要:分析外墙外保温系统瓷砖饰面瓷砖脱落的因素,研制适用于瓷砖饰面保温系统的高性能填缝剂。该填缝剂配比为:粉煤灰25%等量取代水泥,纤维素醚HEMC掺量0.2%,有机硅改性可再分散胶粉VC/E/VL掺量1.5%,硅烷基粉末憎水剂掺量0.3%,高铝水泥掺量为水泥与粉煤灰总量5%。按此配比配制的填缝剂粘结性能、抗折强度、压折比、吸水量、收缩值等指标均符合JC/T1004—2006标准要求。By analyzing the factors of long-term off of ceramic tiles of the exterior insulation system,flexible hydrophobic mortar satisfied the system is developed. The best mix ratio is: 25% fly ash to replace the cement,0. 2% cellulose ether HEMC,1. 5% disperse powder VC / E / VL of organic silicon modified,0. 3% silane-based water repellent,5% alumina cement by the total of cement and fly ash. The performance indicators of bonding,flexural strength,ratio of compressive strength to flexural strength,water absorbing capacity,shrinkage of grout prepared by the best ratio are far in line with standard JC / T1004—2006.

关 键 词:填缝剂 粉煤灰 纤维素醚 可再分散胶粉 憎水剂 高铝水泥 

分 类 号:TU522.18[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象