LF炉高效生产实践  被引量:1

Efficient Production Practice on Steelmaking by Ladle Furnace

在线阅读下载全文

作  者:高洪涛[1] 魏元[1] 毛志勇[1] 王鹏飞[1] 徐福泉[1] 

机构地区:[1]鞍钢股份有限公司炼钢总厂,辽宁鞍山114021

出  处:《鞍钢技术》2015年第5期51-53,62,共4页Angang Technology

摘  要:分析了影响鞍钢股份有限公司炼钢总厂四分厂LF炉高效生产的原因,通过采取进LF炉钢水温度大于1 590℃、硫含量不超过0.024%、LF炉前期温度控制稍高、合理减少加铝批次等措施后,普碳钢的LF炉处理周期大约缩短4 min。The reasons for influencing the efficient production practice on steelmaking by ladle furnace in No.4 Branch of General Steelmaking Plant of Angang Steel Co., Ltd. are analyzed.After taking such measures as increasing the temperature of molten steel poured into the ladle furnace more than 1 590 ℃, controlling the content of sulphur up to 0.024%, adjusting the temperature of molten steel to a little bit higher than the traditonal temperature before pouring the ladle furnace and suitably reducing the heat of adding aluminium, the steelmaking period of common carbon steel by ladle furnace is shortened by about 4 minutes.

关 键 词:LF炉 处理周期 钢水温度 

分 类 号:TF748[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象