核桃壳骨架构建剂对污泥脱水性能的影响  被引量:10

Walnut shell used as skeleton builder for improving sludge dewatering properties

在线阅读下载全文

作  者:董凌霄[1] 丁绍兰[1] 谢林花[1] 蔡丽[1] 杨慧佳[1] 

机构地区:[1]陕西科技大学资源与环境学院,西安710021

出  处:《环境工程学报》2016年第1期365-369,共5页Chinese Journal of Environmental Engineering

基  金:陕西科技大学资助项目(2012SB042)

摘  要:污泥最终处置的困难在于提高泥饼的含固量和降低其含水率。研究用核桃壳做骨架构建剂对污泥进行调理对污泥脱水性能改善的影响。通过测定污泥比阻(SRF),毛细吸水时间(CST)以及抽滤后污泥含水率,探究核桃壳骨架构建剂对污泥脱水性能的影响。结果表明,采用核桃壳做骨架构建剂调理污泥的最佳添加量为4∶6(核桃壳与污泥干重比),最佳粒径为<0.25 mm。用真空抽滤脱水,核桃壳调理后污泥的含水率明显降低。含水率为97.5%的原泥经过29 min真空抽滤后泥饼含水率降至70.52%;按核桃壳与污泥干重比4∶6,添加粒径<0.25 mm的核桃壳后,泥饼含水率降为63.57%,SRF由初始的3.73×1013m/kg,降为调理后的1.06×1013m/kg。It was well known that the main difficulty in sludge disposal was to increase the solids content and decreasing water content. In the study,the sludge dewatering properties were investigated when it was conditioned with walnut shell used as skeleton builder. During the course of experiment,some parameters such as sludge resistance of filtration( SRF),capillary suction time( CST) and water content of sludge cake were monitored. The experimental results showed that the best ratio of walnut shell and sludge mass( dry weight) was 4 ∶ 6,the best suitable walnut shell particle was 0. 25 mm. Water content of sludge cake conditioned with walnut shell decreased greatly when it was dewatered by vacuum pump. When the raw sludge with 97. 5% water content was filtrated for 29 min with vacuum pump,the water content of sludge cake decreased to 70. 52%. When conditioned with walnut shell whose particle size was 0. 25 mm according to the ratio of 4 ∶ 6( ratio of dry weight),water content of sludge cake decreased to 63. 57%. The values of SRF decreased from 3. 73 × 10^13 m / kg in the original to 1. 06 × 10^13 m / kg conditioned with walnut shell.

关 键 词:核桃壳 骨架构建剂 脱水性 污泥比阻 毛细吸水时间 

分 类 号:X7[环境科学与工程—环境工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象