机构地区:[1]首钢水城钢铁(集团)有限责任公司技术中心,贵州六盘水553028
出 处:《冶金信息导刊》2015年第6期37-40,共4页Metallurgical Information Review
摘 要:描述了水钢4号高炉炉况波动的过程。通过分析,得知炉况波动的主要原因是烧结矿强度下降所致。认识到烧结工序合理配料结构的重要性,提出了水钢条件下的常用料结构,将烧结矿强度与焦炭强度同等对待。The working condition fluctuation process of No.4 blast furnace in Shuigang is described in this article. Through the analysis of the furnace condition fluctuation, it finds that the main cause is a decrease in sintering ore strength. Realizing the importance of reasonable burden structure in sintering process, favorable burden structure under the condition of Shuigang is put forward. Meanwhile, it should emphasis on the sintering ore strength as same as the coke strength.