00Cr22Ni5Mo3N双相不锈钢在某气田雅丹地貌土壤中的腐蚀行为  

Corrosion Behavior of 00Cr22Ni5Mo3N Duplex Stainless Steel in Yardang Soil

在线阅读下载全文

作  者:李循迹[1] 周理志[1] 常泽亮[1] 孟祥娟[1] 宋文文[1] 

机构地区:[1]中国石油塔里木油田分公司,新疆库尔勒841000

出  处:《材料保护》2016年第4期59-61,8,共3页Materials Protection

摘  要:为考察00Cr22Ni5Mo3N双相不锈钢在中国西部某气田雅丹地貌环境的腐蚀行为及对其施加阴极保护的必要性,采用现场埋设试片的方法,通过对试片的腐蚀速率、腐蚀形貌分析,研究了其腐蚀行为特征。结果表明:00Cr22Ni5Mo3N试片在该土壤中的平均腐蚀速度低,适用于该气田集气管线,并无施加阴极保护的必要性。In order to evaluate the corrosion behavior of 00Cr22Ni5Mo3 N duplex stainless steel in Yardang soil of gas field located in West China and the necessity of cathodic protection,the characteristics of corrosion behavior were studied by analyzing the corrosion rate and corrosion morphology of sample using coupon tests.Results showed that the average corrosion rate of 00Cr22Ni5Mo3 N sample in the soil was low,which indicated that the sample was suitable for gas-gathering line in gas filed and there was no need to take cathodic protection.

关 键 词:00Cr22Ni5Mo3N双相不锈钢 腐蚀行为 雅丹地貌 气田 腐蚀速率 阴极保护 

分 类 号:TE980.1[石油与天然气工程—石油机械设备] TG174.4[金属学及工艺—金属表面处理]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象