提高温度对ZL102锶变质效果的影响  

Effects of Elevated Temperature on Sr Modified ZL102 Alloy

在线阅读下载全文

作  者:赵岩[1,2] 侯晓霞[1,2] 

机构地区:[1]德州学院机电工程学院,山东德州253023 [2]德州学院工程材料研究所,山东德州253023

出  处:《热加工工艺》2016年第3期96-97,106,共3页Hot Working Technology

基  金:山东省科技发展计划项目(2011YD03099)

摘  要:采用Al-10%Sr,在800℃下对ZL102进行变质处理,获取了变质剂的加入量及保温时间对ZL102铸态力学性能的影响。总体上看,与740℃下的变质相比,变质效果的变化趋势相似,随保温时间延长先升高后下降,但最佳变质效果明显变差。ZL102采用Al-10%Sr变质处理的最佳保温时间在30 min左右,提高温度对于净化改善合金液具有重要作用。The effects of Al-10%Sr addition and holding time on as-cast mechanical properties of ZL102 alloy at 800℃ were investigated. The modification effect as a whole increases firstly and then decreases with extension of holding time, which is similar with the modification effect at 740℃. But the best modification effect is deteriorated obviously. The optimum holding time for ZL102 modified by Al-10%Sr is about 30 min. The elevated temperature plays an important role in purifying and improving alloy melting.

关 键 词:ZL102 锶变质 高温 变质效果 

分 类 号:TG292[金属学及工艺—铸造]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象