转炉冶炼焊条钢留渣操作实践  

PRACTICE OF CONVERTER SLAG- REMAININGOPERATION IN SMELTING ELECTRODE

在线阅读下载全文

作  者:李硕 王振刚 刘善喜 张垚 张虎成 

机构地区:[1]河北钢铁集团唐钢长材部

出  处:《河南冶金》2016年第1期23-25,共3页Henan Metallurgy

摘  要:通过留渣实践表明:较佳的渣量范围3.2 t^3.6 t,配合"高拉补吹"操作,可以提高转炉终点脱磷率由87.4%至89.7%,首次拉碳磷含量由0.0244%下降至0.0178%,终点氧含量由849.6×10-6降低至611.2×10-6,显著降低了冶炼成本。The study on the relationship between slag- remaining amount and efficiency of dephosphorization is carried out,ferrous charges consumption show that controlling the slag- remaining amount in 3. 2t to 3. 6t can enhance the dephosphorization efficiency from 87. 4% to 89. 7%. Slag- remaining operation is used to improve the efficiency of dephosphorization,the phosphorus content of blowing end- point decreases from 0. 0244% to 0. 0178%. The operation of catching carbon and reblowing is used to enhance the control precision of the end- point composition and temperature,the average end- point oxygen content decreases from 849. 6 × 10- 6 to 611. 2 × 10- 6,the smelting cost reduce significantly.

关 键 词:留渣 焊条 氧含量 

分 类 号:TF713[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象