工业锅炉低温腐蚀研究  被引量:3

Study on Low-temperature Corrosion of Industrial Boiler

在线阅读下载全文

作  者:陆倩[1] 

机构地区:[1]江苏省特种设备安全监督检验研究院南通分院,南通226001

出  处:《中国特种设备安全》2016年第6期60-63,共4页China Special Equipment Safety

摘  要:随着锅炉节能要求日趋严格,锅炉排烟温度降低,尾部低温受热面腐蚀严重。本文通过理论公式计算,研究燃料类型、过量空气系数以及燃料含硫量对酸露点温度的影响,确定燃料含硫量对酸露点温度影响最为明显,硫元素含量下降2%,酸露点温度下降30℃以上。因此,燃料脱硫与防腐材料的合理利用,可以在保证合理的排烟温度和锅炉条件下,避免低温腐蚀发生。With the increasing requirements of boiler energy saving, the flue gas temperature was reduced, and the low temperature corrosion in tail heating surface was serious. In this paper, the influence of fuel type, excess air ratio and fuel sulfur content on the dew point temperature was researched by theoretical formula. It was pointed that the fuel sulfur content could significantly affect acid dew point temperature. If the sulfur content decreased 2%, the acid dew point temperature dropped more than 30℃ . Therefore, the rational use of fuel desulfurization and anticorrosion material, can avoid low temperature corrosion under the reasonable condition of exhaust temperature.

关 键 词:低温腐蚀 酸露点 燃料脱硫 耐腐材料 

分 类 号:X933.2[环境科学与工程—安全科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象