作 者:刘媛[1] 卢翠香[1] 苏勇 王建忠 兰俊 陈健波[1]
机构地区:[1]广西林业科学研究院广西优良用材林资源培育重点实验室国家林业局中南速生材繁育实验室,广西南宁530002 [2]广西国有东门林场,广西扶绥532108
出 处:《桉树科技》2016年第2期39-43,共5页Eucalypt Science & Technology
基 金:广西林业科技项目(桂林科字[2013]第1号);广西林业科技项目(桂林科字[2015]第44号);广西林业科技项目(桂林科字[2014]第20号);广西优良用材林资源培育重点实验室自主课题(14-A-02-03);基本科研业务费专项(林科201414号)
摘 要:采用百度试验法研究26年生大花序桉木材的干燥特性。结果表明:大花序桉木材初期开裂严重,缺陷等级达4级;截面变形程度2级;内部开裂程度中等,为2级;干燥速度较慢,为5级。根据木材干燥特性结果,参照百度试验缺陷等级以及干燥缺陷对应的干燥条件,制定了26年生大花序桉木材干燥基准。Drying characteristics of 26-year-old Eucalyptus cloezianawood were examined using the 100 oC test method. Results showed that in wood of E. cloeziana: initial checks were serious and categorized as Grade 4; the degree of cross-section deformation was moderate and categorized as Grade 2; internal checks were also moderate and categorized as Grade 2; drying was slow and categorized as Grade 1. Based on the results obtained on the wood drying characteristics, a drying schedule for E. cloezianajuvenile wood wasproposed based drying conditions necessary to minimize drying defects.
分 类 号:S781.71[农业科学—木材科学与技术]