脱汞载硫活性炭的制备及表征  

Preparation and Characterization of Sulfur-loaded Activated Carbon for Mercury Removal

在线阅读下载全文

作  者:范莉莉[1] 刘晓玲[1] 刘霞[1] 

机构地区:[1]银川能源学院,宁夏银川750105

出  处:《皮革与化工》2016年第4期31-34,共4页Leather And Chemicals

基  金:银川能源学院科研基金项目;项目编号2015-KY-Y-06

摘  要:本文以太西煤基活性炭为载体,研究了载硫活性炭的制备工艺,并探讨了四氯化碳吸附值、S/C和浸渍时间对载硫量的影响,同时采用BET表征对制备的载硫体的结构进行了表征。结果表明:当四氯化碳吸附值为60%,S/C为14%,浸渍时间为24h时,所制备的载硫活性炭载硫量最高为10.89%,且溶剂回收率高达90%。In this paper, the preparation of sulfur-loaded activated carbon was studied,Taixi Coal Based-Activated Carbon used as the carrier. Some factors were discussed such as the carbon tetrachloride adsorption, S/C and dipping time on the influence of amount of sulfur. Meantime the structure of the prepared carrier was characterized by BET. The results showed that: when the carbon tetrachloride adsorption value was 60%, S/C was 14%, and the time was 24h, the sulfur content of the prepared activated carbon was 10.89%, and the solvent recovery rate was 90%.

关 键 词:活性炭 载硫活性炭 载硫量 脱汞 

分 类 号:TQ424.1[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象