Uranium Bioleaching from Low Grade Uranium Ore in Shake Flask

在线阅读下载全文

作  者:王俊[1] 王学刚[1] 孙占学[1] 刘亚洁[1] 张凯钧[1] WANG Jun WANG Xue-gang SUN Zhan-xue LIU Ya-jie ZHANG Kai-jun(State Key Laboratory Breeding Base of Nuclear Resources and Environment, East China Institute of Technology, Nanchang 330013, China)

机构地区:[1]东华理工大学核资源与环境省部共建国家重点实验室培育基地,南昌330013

出  处:《有色金属(冶炼部分)》2016年第10期33-35,47,共4页Nonferrous Metals(Extractive Metallurgy)

基  金:国家自然科学基金资助项目(51564001);科技部国际合作项目(2011DFR60830);江西省教育厅科技落地计划项目(KJLD14048)

摘  要:对某铀矿山低品位铀矿石开展了不同矿浆浓度的细菌浸出摇瓶试验。在相同浸出条件下,经90h浸出,10%、20%、30%和40%矿浆浓度的铀浸出率分别为77.76%、76.20%、60.04%和35.85%,通过适度控制矿浆浓度可以维持比较好的铀浸出效率。Low grade uranium ore was bioleached in shake flask under different pulp concentration. Uranium leaching rate is 77.76%, 76.20%, 60.04%, and 35.85% respectively with pulp concentration of 10%, 20%, 30%, and 40% respectively after bioleached for 90 h under the same conditions. Reasonable leaching efficiency of uranium can be maintained by controlling appropriate pulp concentration.

关 键 词:低品位铀矿石 矿浆浓度 细菌浸出 摇瓶 

分 类 号:TL212.12[核科学技术—核燃料循环与材料]

 