低钛型钒钛磁铁矿深度还原-磨选分离试验  被引量:6

Experimental Research on Deep Reduction and Grinding Separation of Low Ti-bearing Vanadium-titanium Magnetite

在线阅读下载全文

作  者:李菊艳[1] 唐恩[1] 秦涔[1] 周强[1] 范小刚[1] 王君[1] 

机构地区:[1]中冶南方工程技术有限公司,湖北武汉430223

出  处:《钢铁钒钛》2016年第5期25-29,共5页Iron Steel Vanadium Titanium

摘  要:对某低钛型钒钛磁铁矿进行深度还原-磨选分离试验,结果表明:还原温度1 050℃,还原时间10 h,是抑制钒还原的临界条件;使用添加剂和延长还原时间能够强化钒钛磁铁矿还原,其中硼砂能够有效促进钒钛磁铁矿还原,硼砂用量3%时,产物金属化率达98.21%,而Ca F2在本试验条件下对还原起到抑制作用,弱磁选并深度细磨有利于铁、钒分离。Experimental research on deep reduction and grinding separation of a certain low Ti-bearing vanadium-titanium magnetite was conducted. The results show that the critical conditions for inhibiting the reduction of vanadium are reduction at 1 050 ℃ for 10 h. The reduction of vanadium-titanium magnetite can be enhanced by additives and extension of reduction time. Borax can efficiently promote the reduction of the vanadium-titanium magnetite, and the metallization rate of product reaches 98.21% with 3% borax added. However, inhibitory effects on reduction were observed with CaF2 in the experiments. Low intensity magnetic separation and deep grinding are beneficial to separate Fe and V.

关 键 词:钒钛磁铁矿 深度还原 磁选分离 提钒 

分 类 号:TF841.3[冶金工程—有色金属冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象