厚规格管线钢卷形缺陷成因分析及改进  被引量:11

Analysis and improvement of the coil shape defects of thick gauge pipeline steel

在线阅读下载全文

作  者:王章岭[1] 陈彤[1] 田贵昌[1] 韩乐[1] 王莉[1] 刘建华[1] WANG Zhang-ling CHEN Tong TIAN Gui-chang HAN Le WANG Li LIU Jian-hua(Shougang Jingtang United Iron ~ Steel Co. , Ltd. , Tangshan 063200, Chin)

机构地区:[1]首钢京唐钢铁联合有限责任公司,河北唐山063200

出  处:《轧钢》2016年第5期78-81,共4页Steel Rolling

摘  要:针对厚规格管线钢卷取过程中出现的不同卷形缺陷,从设备精度、侧导板短行程控制、侧导板纠偏功能、夹送辊辊缝设定等方面进行了分析和优化。通过有针对性地采取措施进行改进后,有效降低了卷形缺陷发生率,提高了卷形一次命中率和卷形质量,增强了企业市场竞争力和客户满意度。Aimed at the different coil shape defects of thick gauge pipeline steel in the coiling process,the equipment precision,side guide short stroke control,side guide corrective functions,pinch roll gap setting were analyzed and optimized.Taking some targeted measures,the incidence of coil shape defects was reduced effectively,and the first-hit yield and the coil quality were improved,also the customer satisfaction and market competitiveness were upgraded.

关 键 词:管线钢 厚规格 卷形缺陷 工艺控制 

分 类 号:TG335.11[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象