作 者:李刚[1] LI Gang(Liaoning Province Building Science Research Institute, Shenyang 110005, China)
出 处:《低温建筑技术》2017年第4期12-14,共3页Low Temperature Architecture Technology
摘 要:研究渗透结晶型抗裂防水剂对混凝土性能的影响,主要研究了工作性、电通量、早期抗裂性等性能指标。试验结果表明:混凝土中掺入渗透结晶型抗裂防水剂后,不影响混凝土的工作性,减水剂掺入0.75%时,掺入抗裂防水剂混凝土的坍落度达到160mm;掺入抗裂防水剂后混凝土90d电通量较28d下降了48.2%,同时掺入抗裂防水剂混凝土抗早期抗裂性比未掺抗裂防水剂的混凝土要好。This paper has studied the effect of the permeable crystalline type anti-cracking water- proofing agent on the performance of the concrete. Some primary performance indexes about the con- cretes, such as the workability, the electric flux and the early cracking resistance were analyzed. The testing results show that the addition of the permeable crystalline crack resistant waterproofing agent has no effect on the workability of the concrete. When the content of the water-reducing admixture is 0.75% , the slump of concrete added with anti-cracking waterproofing agent reaches 160mm. The elec- tric flux of the concrete after curing for 90 days is 48.2% lower than that of 28 days. Additionally, the cracking resistance of the concrete with the addition of anti-cracking waterproofing agent was better than that of the concrete without the addition at early age.
关 键 词:渗透结晶 抗裂防水剂 工作性 电通量 早期抗裂性
分 类 号:TU528.0[建筑科学—建筑技术科学]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:18.191.158.217