再生粗骨料取代率对再生保温混凝土抗压强度离散性影响  被引量:9

Influence of Recycled Coare Aggregate Replacement Rate on the Discreteness of the Compressire Strength of Recycled Aggregate Thermal Insulation Concrete

在线阅读下载全文

作  者:赵雨[1] 刘元珍[1] 王文婧[1] 郭耀东[1] 

机构地区:[1]太原理工大学建筑与土木工程学院,太原030024

出  处:《科学技术与工程》2017年第13期275-279,共5页Science Technology and Engineering

基  金:国家自然科学基金(51508370;51678384)资助

摘  要:对再生保温混凝土(简称为RATIC)的抗压强度和抗压强度离散性的规律进行了分析。通过改变RATIC中再生粗骨料的取代率,对比分析不同再生粗骨料取代率对RATIC的抗压强度和离散性的影响;并且探索出其相应的规律。以再生粗骨料不同取代率为基础的研究试验发现:当再生粗骨料取代率为30%时,RATIC抗压强度相对于取代率为0%的保温混凝土的抗压强度值没有发生显著变化;当再生粗骨料取代率在30%以上时,随着再生粗骨料取代率的增加,RATIC抗压强度值出现明显下降的现象;当再生粗骨料取代率达到70%时,相对应的RATIC抗压强度出现最低值。与此同时,RATIC在不同再生粗骨料取代率对应下的抗压强度标准差值的波动幅度也较为明显;当再生粗骨料取代率在0~100%时,RATIC的抗压强度标准差在0.97~1.71 MPa之间变化;并且当再生粗骨料取代率为50%时,RATIC抗压强度标准差达到最大值1.71 MPa。The analysis and introducing rule about compressive strength and discreteness of thermal insulation concrete with recycled aggregates( RATIC) were maken. By change the replacement proportion of recycled coarse aggregate of RATIC, the impact about the different replacement proportion of recycled coarse aggregate for compressive strength and discreteness of RATIC and explore its rule were comparatively analysed. The findings under different replacement proportion of recycled coarse aggregate the conpressive strength different is not big between RATIC and TIC when the replacement proportion is thirty percent. When the replacement proportion above thirty percent,the compressive strength of RATIC significantly decreased with the increment of replacement proportion when replacement proportion of recycled coarse aggregate change; When the replacement proportion of recycled coarse aggregate reach seventy percent,compressive strength of RATIC reach the lowest level; Meanwhile,compressive strength standard deviation change significantly of RATIC with the different replacement proportion of recycled coarse aggregate,when the replacement proportion of recycled coarse aggregate between zero percent and one hundred percent,the compressive strength standard deviation of RATIC between 0. 97 MPa and 1. 71 MPa,and when the replacement proportion of recycled coarse aggregate reach fifty percent,compressive strength standard deviation of RATIC reach the largesy level,this value is 1. 71 MPa.

关 键 词:再生保温混凝土 再生粗骨料取代率 抗压强度 标准差 

分 类 号:TU528.79[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象