±800kV特高压输电线路耐张线夹未压区鼓胀缺陷分析  被引量:5

Analysis on Bulge Defect of Strain Clamp of ±800 kV Extra-high Voltage Transmission Lines

在线阅读下载全文

作  者:吴坤祥[1] 朱迪锋 许杨勇[1] 谭益民[1] 刘红鑫[1] 

机构地区:[1]国网浙江省电力公司检修分公司,杭州311232

出  处:《浙江电力》2017年第7期11-13,28,共4页Zhejiang Electric Power

摘  要:针对某±800 kV输电线路耐张线夹未压区膨胀开裂缺陷,通过宏观检查、解剖分析、渗水试验等综合分析,认为耐张线夹膨胀开裂原因是雨水通过导线线股细微间隙渗入未压区后受冷冰冻膨胀,最终导致耐张线夹膨胀开裂。同时,提出3种耐张线夹更换方案,筛选最优方案进行缺陷消除,并给出运维建议。Through macroscopic examination, anatomical analysis and seepage test, it is believed that the strain clamp bulge and crack of ±800 kV transmission lines was caused by the bulge due to freezing of rain water seeped into line strands, which led to bulge and crack of the strain clamp. Meanwhile, the paper proposes three schemes for strain clamp replacement; besides, it selects an optimal scheme for defect elimination and brings forward operation and maintenance suggestions.

关 键 词:耐张线夹 膨胀开裂 特高压 输电线路 

分 类 号:TM755[电气工程—电力系统及自动化]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象