碱性硫化钠浸出含锑金精矿的试验与工业实践  被引量:7

Experiment and Industrial Practice of Leaching of Antimony-bearing Gold Concentrate with Alkaline Sulfide

在线阅读下载全文

作  者:张大伟[1] 王云[2] 靳冉公[1] 李云[1] 

机构地区:[1]北京矿冶研究总院,北京100160 [2]浙江华友钴业股份有限公司,浙江桐乡314500

出  处:《有色金属(冶炼部分)》2017年第9期1-4,共4页Nonferrous Metals(Extractive Metallurgy)

基  金:国家"十二五"科技支撑计划项目(2012BAB08B04);国土资源部公益性行业科研专项(201211069-02)

摘  要:采用碱性硫化钠浸出—无隔膜电积的方法回收含锑金精矿中的锑,在小型试验基础上根据生产场地的实际情况进行了工业实践。通过对电积过程工艺参数优化,锑综合浸出率为96.72%,回收阴极锑纯度96.36%,贫液含锑5.54g/L,综合电流效率63.84%,吨锑氢氧化钠消耗量617.2kg。Antimony in antimony-bearing gold concentrates was recovered by alkaline sodium sulphide leaching, and segregation-free electrodeposition. Based on small-scale experiment, industrial practice was carried out according to actual conditions of production site. After optimization of process parameters of electrodeposition, comprehensive leaching rate of antimony is 96. 72%, purity of cathode antimony is 96.36%, antimony concentration in barren liquor is 5. 54 g/L, comprehensive current efficiency is 63.84%, and NaOH consumption for one ton antimony is 617.2 kg.

关 键 词:硫化钠 含锑金精矿 阴极锑 电积 

分 类 号:TF818[冶金工程—有色金属冶金]

 