作 者:王中江 刘华侨 李红卫 顾培霜 朱家顺 WANG Zhongjiang LIU Huaqiao LI Hongwei G U Peishuang ZHU Jiashun(Shandong Fengyuan Tire Manufacturing Co. ,Ltd, Zaozhuang 277300, China TTA ( Qingdao ) Tire Technology Co. , Ltd Qingdao 266061, China)
机构地区:[1]山东丰源轮胎制造股份有限公司,山东枣庄277300 [2]特拓(青岛)轮胎技术有限公司,山东青岛266061
出 处:《橡胶工业》2017年第10期615-619,共5页China Rubber Industry
摘 要:试验研究溶聚丁苯橡胶(SSBR)牌号切换对轮胎硫化胎面接头缺胶的影响。研究表明,在半钢子午线轮胎胎面体系中,以SOL 6270M等量替换RC2557S,若保证胎面胶门尼流变等加工性能,则流动性下降,引起胎面接头缺胶。通过调整混炼工艺,提高胶料的流动性,成品轮胎硫化外观得到有效改善。The effect of SSBR brand transition on the tread joint cracking was studied. The test results showed that use of SOL 6270M to replace RC2557S in the tread recipe of steel belted radial tire resulted in the decline of flow property at a similar level of Mooney viscosity,which caused tread joint cracking.By adjusting the mixing process to improve the fluidity,the appearance defects of the finished tire were effectively avoided.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.15