摘  要:总结细号棉纱与Coolcool纤维交织物的生产要点。以4.2tex×2精梳纯棉股线为经纱;以166.5dtex的Coolcool长丝包覆44.4dtex的氨纶长丝组成的弹力网络丝为纬纱,生产了一款小提花织物;介绍了络筒、整经、浆纱、织造和后整理各工序的工艺要点和采取的技术措施。最终保证了产品的顺利生产,织机效率达88%以上,十万纬经停4.4次,十万纬纬停9.6次,下机一等品率86.5%。认为:生产的织物细腻滑爽,吸湿透气,可用作高档衬衫面料。Production key points of fine cotton yarn and Coolcool fiber interweave tabric was summarized. 4. 2 texX 2 combed cotton ply was used as warp, elastic interlaced yarn as weft which was composed of 166.5 dtex Coolcooi fiber filament covered with 44.4 dtex spandex filament, a kind of mini-jacquard fabric was produced. Technology points and technology measures in winding, warping, sizing, weaving and after-finish were introduced. Finally the smooth production was ensured. Loom efficiency is above 88G. Warp stop times per 100 000 weft is 4.4. Weft stop times per 100 000weft is 9.6. The first grade percentage before cloth repairing is up to 86.5%. It is considered that p-odueed fabric is soft & comfort and b.as better hygroscopicity & permeability. It can be used as high-grade shirting fabric.

关 键 词:长绒棉 Coolcool纤维 络筒机 整经速度 浆料配方 喷气织机 后整理 

分 类 号:TS106.591[轻工技术与工程—纺织工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象