三元复合材料K8[Fe(H2O)W11MnO39]/PANI/TiO2的制备及光催化性能  被引量:5

Preparation and photocatalytic activity of ternary composite materials K8[Fe(H2O)W11MnO39]/PANI/TiO2

在线阅读下载全文

作  者:单秋杰[1] 王静[1] 刘璐[1] 陈伟[1] 田景芝[1] 

机构地区:[1]齐齐哈尔大学化学与化学工程学院

出  处:《分子科学学报》2018年第1期82-88,共7页Journal of Molecular Science

基  金:黑龙江省自然科学基金重点资助项目(ZD201318)

摘  要:采用静电自组装法制备出三元复合材料K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2.采用IR,UV,XRD,SEM,XPS和N2吸附-脱附的表征手段对K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2进行表征,并以龙胆紫为模型,在紫外光照射下,考察了K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2对龙胆紫染料的光催化性能,确定光催化最佳条件:龙胆紫溶液浓度为5mg/L,pH=3,K8[Fe(H2O)W11MnO39]/PANI/TiO2的用量为10mg,脱色率可达92.93%.The ternary composite material of K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2 was synthesized by electrostatic self-assembly method,and was characterized by IR,UV,XRD,SEM,XPS and N2 adsorption-desorption.The photocatalytic activity of K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2 was studied for photocatalytic degradation of gentian violet as a model under the condition of UV irradiation and the optimum experimental reaction conditions of photocatalytic degradation were determined.The results indicated that the concentration of gentian violet solution was 5 mg/L,and the pH of gentian violet solution was 3,and the quantity of K8[Fe(H2O)W(11)MnO(39)]/PANI/TiO2 was 10 mg,and the decolorizing rate reached 92.93% under the best conditions.

关 键 词:三元复合材料 二氧化钛 龙胆紫 光催化 

分 类 号:O649[理学—物理化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象