作 者:郭陈勇 张瀛[2] 浦承皓[2] 张成 石养鑫 魏侃 GUO Chenyong1,ZHANG Ying2,PU Chenghao2,ZHANG Cheng1,SHI Yangxin1,WEI Kan1(1.Xi'an United Pressure Vessel Co., Ltd., Xi'an 710201, China;2.Nuclear and Radiation Safety Center, Beijing 100082, Chin)
机构地区:[1]西安优耐特容器制造有限公司,西安710201 [2]环境保护部核与辐射安全中心,北京100082
出 处:《无损检测》2018年第3期59-61,共3页Nondestructive Testing
基 金:二○一五年陕西省重大科技创新专项资金资助项目(2015ZKC05-10)
摘 要:针对钛/钢、锆/钢复合板容器设备常因覆层盖板焊缝的微小缺陷造成设备在压力试验时出现微泄漏,而常规单一无损检测方法不易检出或精确定位该焊缝微小缺陷的问题,采用氦气检漏法-荧光渗透法或氨气检漏法-荧光渗透法组合的检测工艺,实现了微泄漏点的精确定位,解决了微泄漏的检测问题。The micro leakage often appears during pressure test of vessels equipment with titanium/steel and zirconium/steel cladding plate because of the tiny defect of the weld of the cover plate.However,the common practice single NDT method is not easy to detect or accurately position the defect.Through demonstration of three kinds of combination detection process,the results show that the helium leak detection-fluorescent penetrant method,as well as the ammonia leak detection-fluorescent penetrant method can realize accurate positioning of micro leakage point,and solve the problem of micro leakage detection.
关 键 词:复合板容器 氦气检漏 氨气检漏 荧光渗透检测 精确定位
分 类 号:TG115.28[金属学及工艺—物理冶金]