彩棉渐变条三层织物的设计及生产  

Design and Production of Three Layers Colored Cotton Fabric with Gradient Strip

在线阅读下载全文

作  者:隋全侠 瞿建新 SUI Quanxia;QU Jianxin(Jiangsu College of Engineering and Technology,Jiangsu Nantong,22600)

机构地区:[1]江苏工程职业技术学院,江苏南通226007

出  处:《棉纺织技术》2018年第7期41-44,共4页Cotton Textile Technology

基  金:江苏高校品牌专业建设工程资助项目(PPZY2015A093)

摘  要:总结彩棉渐变条三层织物的设计与生产要点。选用棕色棉/白棉70/30 14.6tex纱和本白棉14.6tex纱为经纱,织物组织为三层接结组织;采用TS008型络筒机,加工色纱速度设定为700m/min,加工本白棉纱速度设定为840m/min;整经速度700m/min。浆纱机速度控制在50m/min^55m/min,上浆时浸透与被覆兼顾;采用GA718型喷气织机,开口时间310°,后梁高度-1,上机张力1 800N。通过调整各工序工艺,最终织机效率达90%以上。认为:最终生产的织物产品附加值较高,适宜用作婴幼儿服装面料和宝宝包被等。The design and key points of three layer colored cotton fabric with gradient strip were summa- rized. The brown cotton/white cotton 70/30 14.6 tex yarn and raw white cotton 14.6 rex yarn were selected as warp. The fabric texture was three layer binding weave. TS008 winding machine was adopted. The processing speed for colored yarn was set as 700 m/min. The processing speed for raw white yarn was set as 840 m/min. The warping speed was 700 m/min. The sizing speed was controlled among 50 m/min- 55 m/min. Both immersing and covering during sizing were combined. GA718 air-jet loom was used. The shed time was 310°, the back rest height was -1 while the loom tension was 1 800 N. Through adjusting the setting of each processing, the loom efficiency was reached above 90° in the end. It is considered that the final fabric produced has higher value add- ed. It is suitable for the garment material of infant,baby quilt and so on.

关 键 词:彩棉 经纱 纬纱 络筒机 整经速度 上浆率 喷气织机 上机张力 

分 类 号:TS106.55[轻工技术与工程—纺织工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象