Preparation of Sm2O3 and Co3O4 from SmCo magnet swarf by hydrometallurgical processing in chloride media  被引量:5

Preparation of Sm_2O_3 and Co_3O_4 from SmCo magnet swarf by hydrometallurgical processing in chloride media

在线阅读下载全文

作  者:K.Sahoo A.K.Nayak M.K.Ghosh K.Sarangi 

机构地区:[1]CSIR-Institute of Minerals and Materials Technology,Bhubaneswar-751013,Odisha,India

出  处:《Journal of Rare Earths》2018年第7期725-732,共8页稀土学报(英文版)

基  金:supported by Sustainable Technologies for the Utilisation of Rare Earths(SURE),CSC-0132 supported by CSIR,India

摘  要:The recycling of rare earth elements(REE) from end-of-life REE based products is an environment friendly proposition. Waste Sm-Co based permanent magnet generated during machining is a good source for both Sm and Co. In the present study a simpler process of acid leaching at 80 ℃ followed by solvent extraction, oxalate precipitation and calcination is described for producing pure Sm2 O3 and Co3 O4. With either 10 vol% H2SO4 or 15 vol% HCI at 80 ℃ more than 95% Sm and Co are leached in 1 h.Extraction of Sm from sulphate leach liquor with TBP or Aliquat 336 was poor. Although extraction with TOPS-99 is quantitative but Sm from sulphate leach liquor precipitated as Sm2(SO4)3·8 H2O. The chloride leach liquor at an initial pH of 2.5 and with 1.2 mol/L TOPS-99 shows requirement of 4-stages at A:O = 3:2. Stripping with oxalic acid precipitates Sm-oxalate which is calcined at 800 ℃ to produce Sm2 O3. Co3 O4 is recovered from the raffinate through oxalate precipitation followed by calcination at450℃.The recycling of rare earth elements(REE) from end-of-life REE based products is an environment friendly proposition. Waste Sm-Co based permanent magnet generated during machining is a good source for both Sm and Co. In the present study a simpler process of acid leaching at 80 ℃ followed by solvent extraction, oxalate precipitation and calcination is described for producing pure Sm2 O3 and Co3 O4. With either 10 vol% H2SO4 or 15 vol% HCI at 80 ℃ more than 95% Sm and Co are leached in 1 h.Extraction of Sm from sulphate leach liquor with TBP or Aliquat 336 was poor. Although extraction with TOPS-99 is quantitative but Sm from sulphate leach liquor precipitated as Sm2(SO4)3·8 H2O. The chloride leach liquor at an initial pH of 2.5 and with 1.2 mol/L TOPS-99 shows requirement of 4-stages at A:O = 3:2. Stripping with oxalic acid precipitates Sm-oxalate which is calcined at 800 ℃ to produce Sm2 O3. Co3 O4 is recovered from the raffinate through oxalate precipitation followed by calcination at450℃.

关 键 词:SmCo magnet SAMARIUM COBALT TOPS-99 Solvent extraction Precipitation stripping 

分 类 号:O614.337[理学—无机化学] O614.812[理学—化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象