作 者:孙晶 王瑞[1] 孙红玉[2] 徐磊[1] 夏燕茂 SUN Jing;WANG Rui;SUN Hongyu;XU Lei;XIA Yanmao(Tianjin Polytechnic University,Tianjin,300387;Huafang Co.,Ltd.,Shandong Binzhou,256617)
机构地区:[1]天津工业大学,天津300387 [2]华纺股份有限公司,山东滨州256617
出 处:《棉纺织技术》2018年第12期23-26,共4页Cotton Textile Technology
摘 要:研究不同捻系数比对纯棉7.3tex×2股线性能的影响。通过对捻系数为350和390的集聚纺单纱分别反向加捻成股线,并表征了股线在不同捻系数比下的表面形貌、断裂强力、强力不匀率、断裂伸长率和条干不匀率。结果表明,在一定范围内,随着捻系数比的增大,股线的强伸性和条干均有所改善;两种单纱捻系数的股线性能变化趋势相似,但单纱捻系数390的股线整体性能较好;捻系数比在0.3~0.5和1.2~1.5之间时,两种股线性能均较好。The effects of different twist s on the properties condensed yarn with of pure cotton 7. 3 tex ×2 ply and plied with different twist multipliers like surface topography, breaking strength, strength unevenness, breaking elongation and yarn unevenness were evaluated. The test results showed that the strength & elongation and yarn evenness were improved as the increase of twist multiplier ratio within certain range. The change trend of plied with two single yarn twist multipliers were similar. However,the overall
关 键 词:纯棉股线 捻系数比 线密度 力学性能 条干不匀率
分 类 号:TS104.34[轻工技术与工程—纺织工程]