作 者:ZHAOYuxi HEXiaoping
机构地区:[1]RefractoryCorporationofTaiyuanIronandSteel(Group)Co.Shanxi03009,China [2]IronandSteelInstitute,TaiyuanIr
出 处:《China's Refractories》2000年第2期19-22,共4页中国耐火材料(英文版)
摘 要:The influence of the composition of AOD slag on the corrosion of rebonded magnesite-chrome brick has been studied by analyzing the residual bricks at the tuyere zone of AOD .It indicates that the corrosion degree increased with the increase of the basicity of slag and decreased with the increase of the content of MgO ,Cr2O3 and Al2O3 in slag.And the addition of refractories to slag up to satura-tion could decrease the corrosion abiliy of sag.It is important to make a resonable slagmaking rule and ensure the percentage of MgO in slag more than 11wt% for pro-longing the service life of lining.
关 键 词:反应机理 氧化镁 铬砖 三氧化二铬 氧化铬 氩氧脱碳炉渣 精炼炉 炼钢
分 类 号:TF748.05[冶金工程—钢铁冶金] TQ175.71[化学工程—硅酸盐工业]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.171