作 者:林程 汤杰 郑翔睿 奚桢浩[1,2] 赵玲[1,2] Lin Cheng;Tang Jie;Zheng Xiangrui;Xi Zhenhao;Zhao Ling(State Key Laboratory of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China;Engineering Research Center of Process System Engineering, East China University of Science and Technology, Shanghai 200237, China)
机构地区:[1]华东理工大学化学工程联合国家重点实验室,上海200237 [2]华东理工大学过程系统工程教育部工程研究中心,上海200237
出 处:《化学反应工程与工艺》2017年第3期205-214,共10页Chemical Reaction Engineering and Technology
基 金:国家重点研发计划(2016YFB0303001);中央高校基本科研业务费重点科研基地创新基金(222201717014)
摘 要:为加深对聚己二酰己二胺(尼龙66)缩聚过程的理解,指导尼龙66生产过程的优化和新工艺开发,本研究基于聚合反应特性以及反应器流体力学特征,耦合聚合反应动力学模型、水-聚合物体系的汽液平衡模型以及传质模型,建立了尼龙66连续缩聚过程管式反应器和后缩聚反应器的数学模型,实现了尼龙66连续聚合过程的模拟。聚合物分子量及水含量的模拟值符合工业生产数据,验证了模型的可靠性,模拟分析了聚合工艺参数对聚合物分子量及水含量的影响,结果表明减少醋酸含量、提高反应器温度、降低管式反应器和后缩聚反应器压力均有利于快速提升聚合物分子量。较优的工艺条件为后缩聚器温度280~285℃,卧管式反应器压力1.600~1.750MPa。建立的模型准确性好,可用于考察工艺参数的影响,指导工业应用。This research is to deepen the understanding of the polycondensation process of polyhexamethylene adipamide(nylon66)and guide the optimization of nylon66production process and development of new technology.Based on the polymerization characteristics and hydrodynamic characteristics of the reactor,the kinetic model of the coupled polymerization,the vapor-liquid equilibrium and mass transfer models of the water-polymer system,the mathematic model of nylon66continuous polycondensation process tubular reactor and post-polycondensation reactor was established,and the simulation of nylon66continuous polymerization was realized.The simulation results indicated that the molecular weight and water content of the polymer were in good accordance with the industrial production data.The reliability of the model was verified and the influence of the polymerization parameters on the molecular weight and water content of the polymer was simulated The results demonstrated that reducing the HAc content,increasing the reactor temperature,reducing the reactor pressure of the tubular and the post-polycondensation reactors were beneficial to rapidly increase the molecular weight of the polymer.The optimum process conditions were post-reactor temperature of280-285oC,the horizontal tubular reactor pressure of1600-1750kPa.The established models were good accuracy and can be used to examine the effects of process parameters and guide industrial applications.
分 类 号:TQ323.6[化学工程—合成树脂塑料工业]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.7