高铁M-3000A无转子硫化仪在TPV动态力学性能方面的应用  

Application of high-speed rail M-3000A MDR in TPV dynamic mechanical properties

在线阅读下载全文

作  者:李长皓 邓涛[1] Li Changhao;Deng Tao(Qingdao University of Science & Technology, Qingdao 266042, Shandong, China)

机构地区:[1]青岛科技大学高分子科学与工程学院,山东青岛266042

出  处:《橡塑技术与装备》2019年第9期52-55,共4页China Rubber/Plastics Technology and Equipment

摘  要:探索了高铁M-3000A无转子硫化仪(MDR)在动态力学方面的应用,得知可用MDR测量定频、定温、定时下的S′(弹性值)、S″(黏性值)、δ(相角)、G′(储能模量)、G″(损耗模量)、Δδ来表征TPV的动态力学性能。结果表明,随动态硫化时间的进行,ACM/TPEE(H55DMG)TPV的S″、δ增大;随S用量的增加,MPU/TPEE(H28DMG)TPV的S′、S″、G′、G″增加,δ和减Δδ减小。The application of high-speed rail M-3000A moving die rheometer (MDR) in dynamic mechanics was explored in this paper. It is known that MDR can be used to measure S'(elastic value), S''(viscosity value),δ(phase angle), G'(storage modulus), G''(loss modulus) and Δδ under fixed frequency, constant temperature and timing, then to characterize the dynamic mechanical properties of TPV. The results show that the S'' and δ of the ACM/TPEE (H55DMG) TPV increased with the progress of the dynamic vulcanization time;As the amount of S increases, S', S'', G', G'' of MPU/TPEE (H28DMG) TPV increased, while δ and Δδ decreased.

关 键 词:无转子硫化仪 动态硫化热塑性弹性体 动态力学性能 

分 类 号:TQ332[化学工程—橡胶工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象