采用海绵钛替代钛铁制备含钛钢的AOD炉冶炼实践  

AOD Furnace Smelting Practice of Using Sponge Titanium to Prepare Titanium-bearing Steel Instead of Titanium Ferrum

在线阅读下载全文

作  者:兰广泽 刘明生[1] Lan Guangze;Liu Mingsheng(No.1 Steelmaking Plant of Shanxi Taigang Stainless Steel Co.,Ltd.,Taiyuan Shanxi030003)

机构地区:[1]山西太钢不锈钢股份有限公司炼钢一厂,山西太原030003

出  处:《山西冶金》2019年第2期92-93,共2页Shanxi Metallurgy

摘  要:基于现有生产线条件,提出了采用AOD炉用海绵钛替换钛铁冶炼含钛钢炉内合金化的方案,通过试验海绵钛收得率比钛铁收得率提高7%左右,减少了AOD合金加入量,可以降低AOD炉氧化终点温度30℃左右,进而减少了高温对耐材的侵蚀。Based on the condition of production line, the scheme of AOD furnace smelting with sponge titanium to prepare titanium-hearing steel instead of titanium fercum is put forward. The yield of titanium sponge is about 7%higher than that of ferrotitanium sponge. By reducing the amount of AOD alloy, the oxidation terminal temperature of AOD furnace can be reduced by about 30 ℃, and the corrosion of refractories at high temperature can be reduced.

关 键 词:含钛钢 AOD炉 海绵钛工艺试验 

分 类 号:TF703[冶金工程—钢铁冶金]

 