出 处:《有色金属》2002年第4期56-58,共3页Nonferrous Metals
摘 要:通过试验 ,研究金属镝冶炼过程中杂质的行为及相应的控制方法。金属镝中的氧、铁、铝主要是由原料引入 ,钙、氟、钨是熔炼过程中进入金属镝的。确保氟化镝原料质量 ,避免铁、铝污染 ,控制合适的工艺条件可以获得高质量的金属镝。在金属钙用量为 9%~ 13 % ,熔炼温度为 14 60℃左右 ,熔炼时间 10~ 2 0min的条件下 ,金属镝的回收率可达 95 %以上 ,进入粗金属镝中的杂质钙、氟。The behavior and control of impurities in dysprosium metal metallurgy are investigated by experiments The impurities in dysprosium metal such as O, Fe and Al are from the raw material dysprosium fluoride, and the Ca, F and W are drawn into dysprosium metal by smelting process The high quality dysprosium metal can be made by control of dysprosium fluoride quality and operation parameters, and avoidance of Fe and Al contamination The recovery of dysprosium is up to 95%, and low contents of Ca, F and W are achieved in the condition of 9%~13% Ca dosage, 1460℃ smelting temperature, and 10~20min retention time
关 键 词:冶炼 金属镝 杂质行为 过程控制 稀土 工艺流程
分 类 号:TF845.3[冶金工程—有色金属冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.28