摘  要:制备了不同配比的乙烯丙烯酸共聚物(EAA)/聚丙烯(PP)共混物,作为三层共挤输液袋内层材料。对材料的介电性能、热性能、力学性能等进行了分析。研究发现EAA添加到PP当中可以提高材料的介电常数,当EAA质量分数为30%的时候,介电常数可以达到4.5,拉伸强度可以达到20.22 MPa,维卡软化温度为121.8℃,同时60 s的焊接剥离强度可以达到44.20 N,基本满足了作为输液袋内层材料的使用条件。The dielectric,thermal and mechanical properties of the three-layer co-extrusion infusion bag were analyzed by using EAA/PP of different proportions as the inner material of the three-layer co-extrusion infusion bag.It is found that the dielectric constant of the material can be increased by adding EAA to PP.When the content of EAA is 30%,the dielectric constant can reach 4.5,and the tensile strength can reach 20.22 MPa,and the Vicat softening temperature is 121.8℃.At the same time,the welding peeling strength of 60 s can reach 44.20 N,which basically meets the requirements as infusion bag inner materials.

关 键 词:高频焊接 输液袋内层 乙烯丙烯酸共聚物 聚丙烯 

分 类 号:TQ3[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象