A3钢薄板激光对接焊工艺研究  

Study on laser butt welding of A3 steel sheet

在线阅读下载全文

作  者:杜洋 赵凯 时云 郝云波 朱忠良 侍倩 DU Yang;ZHAO Kai;SHI Yun;HAO Yunbo;ZHU Zhongliang;SHI Qian(Shanghai Aerospace Equipments Manufacturer Co.,Let.,Shanghai 200245,China)

机构地区:[1]上海航天设备制造总厂有限公司

出  处:《电焊机》2020年第1期75-78,I0008,共5页Electric Welding Machine

基  金:国家自然科学基金青年基金(51705328);上海市青年科技英才扬帆资助项目(17YF1408500)

摘  要:针对A3钢薄板进行连续激光对接焊工艺实验,研究不同工艺参数对焊接成形质量的影响规律。结果表明:随着激光功率的增加,焊接接头熔池宽度、深度及抗拉强度逐渐增加;随着焊接速度的增加,接头熔池宽度、深度降低及抗拉强度逐渐降低;离焦量对接头形貌及拉伸性能影响较小;焊缝间隙小于等于50μm时,接头抗拉强度基本保持不变,可实现有效焊接。Continuous laser butt welding procedure expe-riments were carried out on A3 steel sheet to study the influence of different procedure parameters on the quality of welding.The results show that the width,depth and tensile strength of molten pool of welded joint increase with the increase of laser power.With the increase of welding speed,the width,depth and tensile strength of molten pool decrease gradually.The defocusing amount has little effect on the joint morphology and tensile properties.Effective welding can be achieved by keeping the tensile strength of the joint basically unchanged when the weld gap is below 50μm.

关 键 词:激光对接焊 A3钢 工艺参数 焊缝间隙 

分 类 号:TG456.7[金属学及工艺—焊接]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象