作 者:智茂轩[1] 侯建斌 Zhi Maoxuan;Hou Jianbin(SINOPEC Zhenhai Refining&Chemical Company,Ningbo,Zhejiang,P.C.315207)
机构地区:[1]中国石油化工股份有限公司镇海炼化分公司,浙江宁波315207
出 处:《乙烯工业》2020年第1期60-64,I0002,共5页Ethylene Industry
摘 要:中国石化镇海炼化分公司27 kt/a裂解汽油抽提装置本周期开车以来产品苯乙烯中聚合物含量波动较大,经优化工艺参数、固化现场操作等措施效果有限。最终通过试用新型阻聚剂,并优化调整注入位置有效解决了苯乙烯产品中聚合物含量高的问题,提高了产品质量等级,降低了焦油生成量,实现环保经济效益双赢。The polymer content of styrene product of the 27 kt/a pyrolysis gasoline extraction unit at SINOPEC Zhenhai Refining and Chemical Company has fluctuated greatly since its start-up in this operation cycle,and the effect of measures such as optimizing process parameters and solidifying on-site operation was limited.Finally,the problem of high polymer content of styrene product was effectively solved by trying out new polymerization inhibitor and optimizing injection position,the product quality grade was improved, the tar production was reduced, and both the environmental benefit and economic benefit were achieved.
分 类 号:TE96[石油与天然气工程—石油机械设备]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.3