8Cr4Mo4V异形滚子盐浴软氮化工艺试验  被引量:4

Salt Bath Soft Nitriding Process Test for Special-Shaped Rollers Made of 8Cr4Mo4V

在线阅读下载全文

作  者:刘汇河 宋海涛 姚颖才 李付伟 张艺 LIU Huihe;SONG Haitao;YAO Yingcai;LI Fuwei;ZHANG Yi(Luoyang LYC Bearing Co., Ltd., Luoyang 471039,China;State Key Laboratory of Aviation Precision Bearings, Luoyang 471039, China)

机构地区:[1]洛阳LYC轴承有限公司,河南洛阳471039 [2]航空精密轴承国家重点实验室,河南洛阳471039

出  处:《轴承》2020年第4期15-18,共4页Bearing

摘  要:传统热处理的GCr15异形滚子无法满足使用要求,研究了不同软氮化处理时间对8Cr4Mo4V钢表面硬度、氮化层深度及化合物层深度的影响,结果表明:8Cr4Mo4V滚子的最优软氮化工艺为520℃×18 h,氮化后的滚子工作面硬度及耐磨性得到有效提升,并达到使用寿命。The traditional heat treatment special-shaped rollers made of GCr15 is unable to meet use requirements.The effect of different soft nitriding treatment times on surface hardness of 8Cr4Mo4V steel,depth of nitriding layer and depth of compound layer is investigated.The results show that the optimum soft nitriding process of rollers made of 8Cr4Mo4V is 520℃×18 h.The hardness and wear resistance of working surface of rollers after nitriding are improved effectively,and the service life meet the requirements.

关 键 词:滚动轴承 异形滚子 高温轴承钢 盐浴淬火 软氮化 时间 氮化层深度 表面硬度 

分 类 号:TH133.332[机械工程—机械制造及自动化] TG156.82[金属学及工艺—热处理]

 