降低铅电解阳极泥含铅措施研究  

Study on measures to reduce lead content in anode slime of lead electrolysis

在线阅读下载全文

作  者:黎学坤 LI Xue-kun(Yunnan Chihong resources comprehensive utilization Co.,Ltd,Qujing 655000,China)

机构地区:[1]云南驰宏资源综合利用有限公司,云南曲靖655000

出  处:《世界有色金属》2020年第17期118-119,共2页World Nonferrous Metals

摘  要:通过实验室实验研究,得出在铅阳极泥生产工艺中,1#搅拌桶的控制参数为液固比4~5:1,温度40℃,搅拌时间不少于45min,并且要定期分析铅阳极泥二次洗水成分,通过补入新的生产水来降低溶液铅离子浓度。生产实践表明,按上述参数操作,铅阳极泥铅离子浓度可以控制到14%以下。Through the laboratory experimental research,the control parameters of 1#stirring bucket in the production process of lead anode slime are liquid-solid ratio 4-5:1,temperature 40℃,stirring time no less than 45 min,and the composition of secondary washing water of lead anode slime should be analyzed regularly,and the concentration of lead ion in solution can be reduced by adding new production water.The production practice shows that the lead ion concentration of lead anode slime can be controlled below 14%according to the above parameters.

关 键 词:铅阳极泥 硅氟酸 液固比 铅离子浓度 

分 类 号:TF812[冶金工程—有色金属冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象