国外某难选冶钒钛铁矿石工艺矿物学特征  被引量:10

Process Mineralogical Characteristics of a Foreign Refractory Vanadiumtitanium Iron Ore

在线阅读下载全文

作  者:洪秋阳 李美荣 李波 梁冬云 刘超 张海亮 Hong Qiuyang;Li Meirong;Li Bo;Liang Dongyun;Liu Chao;Zhang Hailiang(Guangdong Institute of Resources Comprehensive Utilization,Guangdong Academy of Sciences State Key Laboratory of Rare Metals Separation and Comprehensive Utilization,Guangdong Provincial Key Laboratory of Development and Comprehensive Utilization of Mineral Resources,Guangzhou,Guangdong,China)

机构地区:[1]广东省科学院资源综合利用研究所,稀有金属分离与综合利用国家重点实验室,广东省矿产资源开发和综合利用重点实验室,广东广州510650

出  处:《矿产综合利用》2020年第6期48-55,共8页Multipurpose Utilization of Mineral Resources

基  金:广东省科学院建设国内一流研究机构行动专项资金项目(2020GDASYL-20200302009);广东省科技计划项目(2017B030314046)。

摘  要:对某钒钛铁矿石进行工艺矿物学研究,分析影响矿石开发利用的矿物学因素。研究结果表明,矿石中的有价元素为钒、钛、铁,杂质元素主要是铝和硅;主要铁、钛矿物分别为磁铁矿-假象赤铁矿-(钛)赤铁矿、褐铁矿和和钛铁矿。铁、钛矿物与脉石连生关系不紧密,且密度、磁性差异较大,易与脉石矿物分离,但是铁、钛矿物之间具有复杂的连生界面,磁性变化大,磁性范围重叠,采用常规磁选工艺难以实现铁、钛的有效分离。采用磁化焙烧-磁选工艺,从磁铁矿-假象赤铁矿-(钛)赤铁矿中回收铁和钒,理论品位为Fe 64.23%和V_2O_5 1.29%,理论回收率分别为60.29%和72.54%;从钛铁矿中回收钛,理论品位为TiO_252.70%,理论回收率为65%左右。Based on the process mineralogy of a vanadium-titanium iron ore,the mineralogical factors affecting the development and utilization of the ore were analyzed.The results show that the valuable elements of the ore are vanadium,titanium and iron,all of which are high grade,and the impurity elements are aluminum and silicon.The main iron and titanium minerals are magnetite-martite-titanohematite,limonite and ilmenite.The iron and titanium minerals are not closely related to gangue,and the density and magnetism are quite different,so they are easy to be separated from gangue.Because of the complicated associated interface between iron and titanium minerals,the variable magnetism and the overlapping magnetism ranges,it is difficult to effectively separate iron minerals from titanium minerals by using conventional magnetic separation processes.By magnetization roasting-magnetic separation process,the theoretical grade of iron and vanadium is Fe 64.23%and V2O51.29%with the theoretical recovery being 60.29%and 72.54%respectively if they are recovered from magnetite-martite-titanohematite,and the theoretical grade of titanium is TiO252.70%with the theoretical recovery being about 65%if the titanium is recovered from ilmenite.

关 键 词: 废催化剂 选钼尾矿 含钼废水 研究现状 展望 

分 类 号:TD952[矿业工程—选矿]

 