纱线质量对喷气织机停台的影响及改进措施  

Impact of Yarn Quality on Stoppage in Air Jet Loom and Improvement Measures

在线阅读下载全文

作  者:赵筛喜[1] ZHAO Shai-xi(Taizhou Polytechnic College,Taizhou 225300,China)

机构地区:[1]泰州职业技术学院,江苏泰州225300

出  处:《纺织科技进展》2021年第2期29-32,共4页Progress in Textile Science & Technology

摘  要:通过测定喷气织机停台状况,统计出经、纬纱纱疵点对喷气织机停台影响的数据。对数据分析可知:纱线毛羽是引起停台的最主要因素,其次分别是细节、大棉结、大杂质、脱节、飞花、大接头等纱疵;提出了改进原纱质量、降低络筒和浆纱毛羽的措施。By measuring the stoppage condition of the air jet loom,the data of the influence of warp and weft yarn defects on stoppage in air-jet loom were obtained.According to the data analysis,yarn hairiness was the most important factor to cause stoppage,followed by the yarn defects such as snicks,big neps,big impurities,self-unknot,flyings and big knot.The measures of improving the quality of the yarn,reducing the winding yarn hairiness and sizing yarn hairiness were put forward.

关 键 词:纱线 质量 喷气织机 停台 措施 

分 类 号:TS112.3[轻工技术与工程—纺织材料与纺织品设计]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象