作 者:文彦博 黄瑞源 李平[2] 马剑[3] 肖凯涛[4] WEN Yanbo;HUANG Ruiyuan;LI Ping;MA Jian;XIAO Kaitao(National Key Laboratory of Transient Physics,Nanjing University of Science and Technology,Nanjing 210094,Jiangsu,China;School of Mechanical Engineering,Anhui University of Technology,Ma'anshan 243032,Anhui,China;Naval Architecture and Civil Engineering,Jiangsu University of Science and Technology,Zhenjiang 215600,Jiangsu,China;Research Institute of Chemical Defense,Beijing 102205,China)
机构地区:[1]南京理工大学瞬态物理国家重点实验室,江苏南京210094 [2]安徽工业大学机械学院,安徽马鞍山243032 [3]江苏科技大学船舶与土木工程学院,江苏镇江215600 [4]防化研究院,北京102205
出 处:《高压物理学报》2021年第2期52-61,共10页Chinese Journal of High Pressure Physics
基 金:国家自然科学基金(11402266,11802001,11672138);中国空气动力研究与发展中心超高速碰撞研究中心开放基金(20200203)。
摘 要:采用∅74 mm大口径分离式霍普金森压杆(SHPB)对不同温度(20、200、400℃)下的C45混凝土材料进行动态力学性能实验,得到了不同温度、不同应变率下混凝土材料的应力-应变曲线。实验结果表明:在20~400℃温度范围内,混凝土材料具有温度硬化和应变率硬化现象。基于上述实验数据给出了损伤变量关于塑性应变的关系式,并通过相关实验数据确定了不同温度、不同应变率下损伤演化方程的材料参数。将该损伤演化方程应用于混凝土材料的本构关系中,预测结果与实验数据具有较好的一致性,证明了所提出的高温、高应变率下混凝土材料损伤演化方程的合理性。In this paper,the dynamic mechanical properties of C45 concrete materials at different temperatures(20,200,400℃)are carried out on split Hopkinson pressure bar(SHPB)equipment with a large diameter of 74 mm.The stress-strain curves of concrete materials at different temperatures and strain rates are obtained through experiments.As the expansion of microcracks inside concrete materials is inhibited by the increase of strain rate,the concrete specimens exhibit strain rate hardening effect.The experimental results show that the concrete material has temperature hardening and strain rate hardening in the temperature range of 20℃ to 400℃.Through the relevant theoretical derivation,the SHPB experimental data of concrete materials are transformed into the relationship between damage variables and plastic strain.Then the material parameters of the damage evolution equation at different temperatures and different strain rates are determined by relevant experimental data.Finally,the damage evolution equation of concrete materials at high temperatures and high strain rates are applied to the constitutive relation of concrete materials.The prediction results are in good agreement with the experimental data.