摘 要:研究了从某低品位氧化铜钴矿石中还原酸浸铜、钴,考察了矿石粒度、反应温度、硫酸用量、还原剂亚硫酸钠用量对铜、钴浸出率的影响。结果表明:在矿石粒度-74μm占80%、液固体积质量比2/1、硫酸用量为矿石质量的8%、还原剂亚硫酸钠用量为矿石质量的12%、反应时间4 h条件下,钴浸出率大于93%,铜浸出率大于95%,浸出效果较好。Leaching of copper and cobalt from a low-grade copper-cobalt oxide ore using sodium sulfite as reducing agent and sulfuric acid as leaching agent was investigated.The effects of ore particle size,temperature,amount of sodium sulfite and sulfuric acid on leaching rate of copper and cobalt were examined.The results show that leaching rate of cobalt and copper are over 93%and 95%,respectively,under the conditions of ore particle size of-74μm accounting 80%,liquid volume-to-solid mass of 2/1,sulfuric acid mass accounting for ore mass of 8%,reducing agent mass accounting for ore mass of 12%,and reaction time of 4 h.
分 类 号:TF803.21[冶金工程—有色金属冶金] TF811
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:18.222.25.95