银层厚度对双银离线Low-E玻璃光热比的影响  被引量:1

The Effect of Silver Layer Thickness on LSG for Double Silver Low-E Glass

在线阅读下载全文

作  者:朱宏刚 ZHU Honggang(Tianjin North Glass Industrial Technical Co.,LTD.,Tianjin 301800,China)

机构地区:[1]天津北玻玻璃工业技术有限公司,天津301800

出  处:《玻璃》2021年第5期52-55,共4页Glass

摘  要:介绍了真空磁控溅射法制备一系列不同银层厚度双银试样,并使用Lambda950和WINDOW6软件测试计算对比每种试样的光热比。实验表明:双银产品的光热比正比于银层总厚度;在总银层厚度相同的情况下第一层银厚度为银层总厚度40%时光热比可获得最大值。本实验为膜层设计人员提高双银膜层光热比提供了一定的参考依据。A series of double silver samples with different silver layer thickness were prepared by vacuum magnetron sputtering.The light heat ratio of each sample was measured and calculated by Lambda950 and windows 6 software.The results show that the light heat ratio is proportional to the total silver layer thickness and the maximum value can be obtained when the first silver layer thickness is 40%of the total silver layer thickness.This experiment provides a reference for film designers to improve the light ratio for double silver film.

关 键 词:太阳能得热因子 光热比(LSG) 双银Low-E 银层比例 

分 类 号:TQ171[化学工程—玻璃工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象