作 者:巢冲 CHAO Chong(Guixi Smelter,Jiangxi Copper Corporation Limited,Guixi 335424,Jiangxi,China)
机构地区:[1]江西铜业集团有限公司贵溪冶炼厂,江西贵溪335424
出 处:《铜业工程》2021年第3期54-57,共4页Copper Engineering
摘 要:优化酸泥浸铅渣中铋的回收工艺,采用硫酸+NaCl为浸出介质,分别研究了各个浸出过程工艺参数的影响,确定了氯盐酸浸最佳工艺参数为:浸出酸度为110 g/L,氯离子浓度为130 g/L,液固比为4∶1,反应温度为85℃,反应时间为2h;中和沉铋最佳工艺参数:pH值为2.5,温度为60℃,时间为1h,可实现酸泥浸铅渣中铋的有效浸出和富集。The recovery process of bismuth in lead slag with sulfuric acid,the influence of the process parameters were studied,and the best process parameters of chloride hydrochloride acid were determined as follows:leaching acidity is 110 g/L,chloride ion concentration is 130 g/L,liquid-solid ratio is 4∶1,reaction temperature is 85℃,reaction time is 2h;the value of the neutralized bismuth:the pH is 2.5,the temperature is 60℃,the time is 1h,which can realize the effective leaching and enrichment of bismuth from the acid sludge leaching lead slag.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.229