珠光体耐热钢顶杆焊接工艺研究  被引量:1

Study on Welding Technology of Pearlitic Heat Resistant Steel Carrier Rod

在线阅读下载全文

作  者:罗玉章 刘健 Luo Yu-zhang;Liu Jian(Steel Tube Co.of Inner Mongolia Baotou Steel Union Co.,Ltd.,Baotou 014010,Inner Mongolia Autonomous Region,China)

机构地区:[1]内蒙古包钢钢联股份有限公司钢管公司,内蒙古包头014010

出  处:《包钢科技》2021年第3期20-22,26,共4页Science & Technology of Baotou Steel

摘  要:12CrMoV珠光体耐热钢顶杆在制作过程中,采用V型坡口焊条电弧焊、水平固定全位置对接接头焊接,焊接性差,焊接难度大,通过规范焊接工艺和焊接质量控制,有效避免了未焊透、夹渣、裂纹等缺陷,保证了焊接质量。In the production process of 12CrMoV pearlitic heat resistant steel carrier rod,there are such problems as poor weldability and great welding difficulty caused by using the v-groove electrode arc welding and horizontal fixed all position butt joint welding,such defects as incomplete penetration,slag inclusion and cracks are effectively avoided by standardizing the welding process and welding quality control to ensure the welding quality.

关 键 词:珠光体耐热钢 夹渣 裂纹 

分 类 号:TG457[金属学及工艺—焊接]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象