连续热镀锌板横向条纹缺陷分析及预防  被引量:1

Analysis and Prevention of Transverse Streak Defects on Continuous Hot dip Galvanized Sheet

在线阅读下载全文

作  者:谢义康 陈德春[1] 施刘健 XIE Yikang;CHEN Dechun;SHI Liujian(Cold Rolling Mill of Maanshan Iron and Steel Co.,Ltd.,Maanshan,Anhui 243000,China)

机构地区:[1]马鞍山钢铁股份有限公司冷轧总厂,安徽马鞍山243000

出  处:《冶金动力》2022年第2期51-52,69,共3页Metallurgical Power

摘  要:连续热镀锌产品板面出现严重横向条纹,通过现场排查并结合理论分析,发现光整机辊系张力控制及精度问题是产生横向条纹的主要原因。采取规范辊系验收,完善相关辊系检查、更换标准、优化辊系使用周期及光整拉矫区域张力优化等措施,可预防类似横向条纹缺陷。It was found that the roller system of the finishing machine was the main cause of the transverse streaks showed on continuous hot-dip galvanized sheets through on site investigation and theoretical analysis.Similar transverse streak defects can be prevented by adopting measures such as standardizing roller system acceptance,improving the relevant roller system inspection/replacement standards,optimizing the use cycle of roller system and optimizing the tension in the finishing and tension leveling area.

关 键 词:热镀锌 横向条纹 张力 稳定性 

分 类 号:TG178[金属学及工艺—金属表面处理]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象