检索规则说明:AND代表“并且”;OR代表“或者”;NOT代表“不包含”;(注意必须大写,运算符两边需空一格)
检 索 范 例 :范例一: (K=图书馆学 OR K=情报学) AND A=范并思 范例二:J=计算机应用与软件 AND (U=C++ OR U=Basic) NOT M=Visual
作 者:翟传田 孙有平[1,2,3] 何江美 孟祥超[1,2] 万斯雨 Zhai Chuantian;Sun Youping;He Jiangmei;Meng Xiangchao;Wan Siyu(School of Mechanical and Automotive Engineering,Guangxi University of Science and Technology,Liuzhou Guangxi 545006,China;Guangxi Earthmoving Machinery Collaborative Innovation Center,Liuzhou Guangxi 545006,China;Guangxi Key Laboratory of Automobile Components and Vehicle Technology,Liuzhou Guangxi 545006,China)
机构地区:[1]广西科技大学机械与汽车工程学院,广西柳州545006 [2]广西土方机械协同创新中心,广西柳州545006 [3]广西汽车零部件与整车技术重点实验室,广西柳州545006
出 处:《金属热处理》2022年第6期39-45,共7页Heat Treatment of Metals
基 金:中央引导地方科技发展专项(2021ZYZX1012);柳州市科技计划(2021CBA0102);广西高等学校高水平创新团队资助项目(桂教师范[2019]52号);广西研究生教育创新计划(YCSW2020221);广西科技大学研究生教育创新计划(GKYC202110)。
摘 要:使用光学显微镜、动态机械热分析仪、X射线衍射仪和扫描电镜研究了不同轧制变形量对Mg-4Zn-2Y和Mg-4Zn-4Y合金显微组织、力学性能及阻尼性能的影响。结果表明,经轧制后合金中出现片层状的LPSO相;两种合金阻尼性能中与应变振幅无关的阻尼性能Q_(0)^(-1)随着轧制变形量的增加,其变化趋势基本一致,与应变振幅相关的阻尼性能Q_(h)^(-1)随着轧制变形量的增加而降低,Mg-4Zn-2Y合金以及Mg-4Zn-4Y合金的阻尼机制为位错型阻尼;随着轧制变形量的增加,合金断口中的韧窝数量增加,解理面减少,主要断裂方式由脆性断裂转变为韧性断裂;相同轧制变形量下,Mg-4Zn-4Y合金的强度优于Mg-4Zn-2Y合金,而阻尼性能要低于Mg-4Zn-2Y合金。Effect of different rolling deformation on microstructure,mechanical properties and damping properties of Mg-4Zn-2Y alloy and Mg-4Zn-4Y alloy was investigated by means of optical microscope,dynamic mechanical thermal analyzer,X-ray diffraction and scanning electron microscope.The experimental results show that the lamellar LPSO phase appears in the alloy after rolling.With the increase of rolling deformation,the change of damping property Q_(0)^(-1) that is independent of strain amplitude is basically the same,and the damping property Q_(h)^(-1) related to the strain amplitude decreases with the increase of rolling deformation.The damping mechanism of the Mg-4Zn-2Y alloy and Mg-4Zn-4Y alloy are the dislocation damping.With the increase of rolling deformation,the number of dimples in the fracture surface of the alloy increases,the dissociation surface decreases,thus the fracture mode changes from brittle fracture to ductile fracture.Under the same rolling deformation,the tensile strength of the Mg-4Zn-4Y alloy is higher than that of the Mg-4Zn-2Y alloy,but the damping capacity is lower than that of Mg-4Zn-2Y alloy.
关 键 词:MG-ZN-Y合金 阻尼性能 轧制变形 力学性能 组织
分 类 号:TG146.4[一般工业技术—材料科学与工程]