HFW焊管沟槽腐蚀研究现状  

Research Status of Groove Corrosion of HFW Welded Pipe

在线阅读下载全文

作  者:王涛 任永峰[1,2] 雒设计 WANG Tao;REN Yongfeng;LUO Sheji(Chinese National Engineering Research Center for Petroleum and Natural Gas Tubular Goods,Baoji 721008,Shaanxi,China;Baoji Petroleum Steel Pipe Co.,Ltd.,Baoji 721008,Shaanxi,China;Xi’an Shiyou University,Xi’an 710065,China)

机构地区:[1]国家石油天然气管材工程技术研究中心,陕西宝鸡721008 [2]宝鸡石油钢管有限责任公司,陕西宝鸡721008 [3]西安石油大学,西安710065

出  处:《焊管》2022年第8期1-9,共9页Welded Pipe and Tube

基  金:中国石油天然气股份有限公司科学研究与技术开发项目“超临界二氧化碳长距离管道关键技术研究”(项目编号2021ZZ01)。

摘  要:为充分了解HFW焊管焊缝沟槽腐蚀机理,及其对高频电阻焊管力学性能的影响,从而探索出有效降低HFW焊管沟槽腐蚀敏感性的方法,从沟槽腐蚀影响规律、测试方法等方面对国内外现阶段沟槽腐蚀研究成果进行分析汇总,着重分析了几种主要的沟槽腐蚀敏感性测试方法,对其优劣性进行了对比。同时,根据沟槽腐蚀研究现状以及相关知识产权的情况,发现目前国内外尚无统一标准的焊缝沟槽腐蚀深度的测量设备或装置,对沟槽腐蚀敏感系数临界值也缺乏工程依据,其失效判定的有效性有待进一步探讨。In order to fully understand the mechanism of HFW welded pipe weld groove corrosion and its influence on the mechanical properties of resistance welded pipe,and explore the methods to effectively reduce the groove corrosion sensitivity of welded pipe,the research results of groove corrosion at home and abroad at this stage are analyzed and summarized from the aspects of groove corrosion impact law,testing methods and so on.Several main groove corrosion sensitivity test methods are emphatically analyzed,and their advantages and disadvantages are compared.At the same time,according to the research status of groove corrosion and relevant intellectual property rights,it is found that there is no unified standard equipment or device for measuring the groove corrosion depth of weld at home and abroad,and there is also a lack of engineering cases for the critical value of groove corrosion sensitivity coefficient,and the effectiveness of its failure determination needs to be further discussed.

关 键 词:HFW焊管 沟槽腐蚀 敏感系数 影响因素 测试方法 

分 类 号:TG174[金属学及工艺—金属表面处理]

 